SPIProduced by the companySPI-Pon ™ eight hundred and twelveEpoxy resin is used to replace those that no longer existEPON 812Epoxy resin. The embedding effect is different from the originalEPON 812Same or even more efficient. withEPON812Similarly, even trace amounts of moisture can affect the performance of the resin. Therefore, in addition to the obvious (the resin cannot fully cure), moisture can cause the formation of bubbles during the polymerization process, resulting in very poor embedding effect.
Microscope technicians often care about the resin viscosity and hardness of the cured block. By using an excessive amount of hardenerSPI-Pon 812It can produce cured blocks that are as hard as all resins, and under these conditions, the resin will polymerize with higher viscosity, resulting in lower potential penetration effectiveness.
Package contents:
l SPI-Pon 812Resin 450ml
l DDSA 450ml
l NMA 450ml
l DMP-30 2*30ml
ordering information:
Item number |
Product Name |
Specifications |
SPI-02660 |
SPI-Pon ™ eight hundred and twelveEpoxy resin embedding reagent kit |
KIT(5 bottles)/Set) |